| Sign In | Join Free | My howtoaddlikebutton.com |
|
Brand Name : lonroy
Place of Origin : Guangdong, China
Model Number : LR-300C
MOQ : 1
Temperature range : -40~600℃
Temperature resolution : 0.001℃
Temperature fluctuation : ±0.001℃
Temperature repeatability : ±0.01℃
Heating rate : 0.1 ~ 80℃/min
Constant temperature time : ≤24h
DSC range : 0 ~ ±600mW
DSC resolution : 0.01uW
DSC sensitivity : 0.001mW
Power supply : AC220V/50Hz or customized
Gas flow : 0-300ml/min
Gas pressure : 0.2mpa
Display type : 7 inch LCD touch screen
Data interface : USB
Cooling device : Semiconductor cooling device (optional liquid nitrogen refrigeration)
| Parameter | Specification |
|---|---|
| Temperature range | -40~600℃ |
| Temperature resolution | 0.001℃ |
| Temperature fluctuation | ±0.001℃ |
| Temperature repeatability | ±0.01℃ |
| Heating rate | 0.1 ~ 80℃/min |
| Constant temperature time | Program setting ≤24h |
| Temperature control mode | Heating, constant temperature, cooling (automatic program control) |
| DSC range | 0 ~ ±600mW |
| DSC resolution | 0.01uW |
| DSC sensitivity | 0.001mW |
| Power supply | AC220V/50Hz or customized |
| Atmosphere control gas | Nitrogen, oxygen (program setting/automatic switch) |
| Gas flow | 0-300ml/min |
| Gas pressure | 0.2mpa |
| Display mode | 24bit color, 7 inch LCD touch screen |
| Data interface | Standard USB interface |
| Parameter standard | Equipped with standard material (indium, tin), user-adjustable temperature |
|
|